SpectraBase Spectrum ID |
enj5C3VAmW |
Name |
E-8353 |
Source of Sample |
Fiberite Corporation |
Chemical Description |
EPOXY MOLDING COMPOUND |
Classification |
POLYMERS - EPOXY RESINS |
Copyright |
Copyright © 1980, 1981-2024 John Wiley & Sons, Inc. All Rights Reserved. |
Deflection Temperature |
(264 PSI) 425F |
Density |
(Specific Gravity)= 1.92-1.95 |
Sample Procedure |
The pyrolysis technique is commonly used in the infrared identification of polymers and results in spectra of both the volatile and non-volatile pyrolyzed fractions the polymer under investigation. It can be used by researchers to identify principal polymer types. The volatile (Vapor Phase) and non-volatile (Condensed Phase) IR spectra resulting from the pyrolysis of this sample are available in SpectraBase as E-8353 - Controlled Pyrolyzate (Vapor Phase) and E-8353 - Controlled Pyrolyzate (Condensed Phase). |
Technique |
KBr WAFER |
Water Absorption |