SpectraBase Spectrum ID |
JpFC3Gr9BKZ |
Name |
CUMAR R-16 (FORMERLY CUMAR MH-2 1/2 RESIN) - Controlled Pyrolyzate (Vapor Phase) |
Source of Sample |
Neville Chemical Company |
Chemical Description |
COUMARONE-INDENE RESIN |
Copyright |
Copyright © 1980, 1981-2024 John Wiley & Sons, Inc. All Rights Reserved. |
Density |
(Specific Gravity)= (25/15.6C) 1.075 |
Fire Point |
(COC) 470F |
Flash Point |
(COC) 412F |
Optical Properties |
Index of Refraction= (25C) 1.5981 |
Sample Procedure |
The pyrolysis technique is commonly used in the infrared identification of polymers and results in spectra of both the volatile and non-volatile pyrolyzed fractions the polymer under investigation. It can be used by researchers to identify principal polymer types. This record contains the volatile (Vapor Phase) IR spectrum resulting from the pyrolysis of CUMAR R-16 (FORMERLY CUMAR MH-2 1/2 RESIN). The IR spectrum of the non-volatile (Condensed Phase) fraction resulting from the pyrolysis of CUMAR R-16 (FORMERLY CUMAR MH-2 1/2 RESIN) is CUMAR R-16 (FORMERLY CUMAR MH-2 1/2 RESIN) - Controlled Pyrolyzate (Condensed Phase). The Temperature in this record is the temperature of the pyrolysis. |
Softening Point |
(RING & BALL) 103C |
Technique |
Vapor Phase |
Values |
Iodine Value= 9 |