SpectraBase Spectrum ID |
JfeTeVES6BL |
Name |
SANDUVOR N-PU |
Source of Sample |
Novartis, Plastics Additives Department |
Chemical Description |
[1-PHENYL 3-METHYL 4-DECANOYL PYRAZOLATE(5)]-NI |
Classification |
MONOMERS - ORGANOMETALLICS |
Copyright |
Copyright © 1980, 1981-2025 John Wiley & Sons, Inc. All Rights Reserved. |
Melting Point |
140-160C |
Sample Procedure |
The pyrolysis technique is commonly used in the infrared identification of polymers and results in spectra of both the volatile and non-volatile pyrolyzed fractions the polymer under investigation. It can be used by researchers to identify principal polymer types. The volatile (Vapor Phase) and non-volatile (Condensed Phase) IR spectra resulting from the pyrolysis of this sample are available in SpectraBase as SANDUVOR N-PU - Controlled Pyrolyzate (Vapor Phase) and SANDUVOR N-PU - Controlled Pyrolyzate (Condensed Phase). |
Technique |
FILM (CAST FROM CHLOROFORM) |