Name EUROPRENE 1707 - Controlled Pyrolyzate (Condensed Phase)
Source of Sample Anic, Milan, Italy
Chemical Description COLD POLYMERIZED OIL-EXTENDED BUTADIENE-STYRENE ELASTOMER
Content Ash Content= 1.00% Bound Styrene Content= 22.5-24.5% Organic Acid Content= 3.90-5.70% Volatile Material Content= 0.75%
Copyright Copyright © 1980, 1981-2024 John Wiley & Sons, Inc. All Rights Reserved.
Dynamic Viscosity (Mooney)= (ML 1+4 100C) 43-58
Sample Procedure The pyrolysis technique is commonly used in the infrared identification of polymers and results in spectra of both the volatile and non-volatile pyrolyzed fractions the polymer under investigation. It can be used by researchers to identify principal polymer types. This record contains the non-volatile (Condensed Phase) IR spectrum resulting from the pyrolysis of EUROPRENE 1707. The IR spectrum of the volatile (Vapor Phase) fraction resulting from the pyrolysis of EUROPRENE 1707 is EUROPRENE 1707 - Controlled Pyrolyzate (Vapor Phase).
Technique Condensed Phase