SpectraBase Spectrum ID |
G0MrRXEEouh |
Name |
ULTEM 2300/1000 - Controlled Pyrolyzate (Condensed Phase) |
Source of Sample |
General Electric Company |
Chemical Description |
GLASS-REINFORCED POLYETHERIMIDE RESIN |
Copyright |
Copyright © 1980, 1981-2024 John Wiley & Sons, Inc. All Rights Reserved. |
Density |
(Specific Gravity)= 1.51 |
Sample Procedure |
The pyrolysis technique is commonly used in the infrared identification of polymers and results in spectra of both the volatile and non-volatile pyrolyzed fractions the polymer under investigation. It can be used by researchers to identify principal polymer types. This record contains the non-volatile (Condensed Phase) IR spectrum resulting from the pyrolysis of ULTEM 2300/1000. The IR spectrum of the volatile (Vapor Phase) fraction resulting from the pyrolysis of ULTEM 2300/1000 is ULTEM 2300/1000 - Controlled Pyrolyzate (Vapor Phase). |
Softening Point |
228C |
Technique |
Condensed Phase |