SpectraBase Spectrum ID |
7kBJP3N1azH |
Name |
ASRC 1712 - Controlled Pyrolyzate (Vapor Phase) |
Source of Sample |
American Synthetic Rubber Corporation |
Chemical Description |
STYRENE-BUTADIENE COPOLYMER |
Content |
Bound Styrene Content= 24.5% MAX
Oil Content= 395 PARTS/100 PARTS R.H.C. MAX |
Copyright |
Copyright © 1980, 1981-2024 John Wiley & Sons, Inc. All Rights Reserved. |
Dynamic Viscosity |
(Mooney)= (ML-4 212F) 40-52 |
Sample Procedure |
The pyrolysis technique is commonly used in the infrared identification of polymers and results in spectra of both the volatile and non-volatile pyrolyzed fractions the polymer under investigation. It can be used by researchers to identify principal polymer types. This record contains the volatile (Vapor Phase) IR spectrum resulting from the pyrolysis of ASRC 1712. The IR spectrum of the non-volatile (Condensed Phase) fraction resulting from the pyrolysis of ASRC 1712 is ASRC 1712 - Controlled Pyrolyzate (Condensed Phase). The Temperature in this record is the temperature of the pyrolysis. |
Technique |
Vapor Phase |