SpectraBase Spectrum ID |
4sUd7WCMmMx |
Name |
EUROPRENE 1707 |
Source of Sample |
Anic, Milan, Italy |
Chemical Description |
COLD POLYMERIZED OIL-EXTENDED BUTADIENE-STYRENE ELASTOMER |
Classification |
POLYMERS - STYRENE-BUTADIENE COPOLYMERS |
Content |
Ash Content= 1.00%
Bound Styrene Content= 22.5-24.5%
Organic Acid Content= 3.90-5.70%
Volatile Material Content= 0.75% |
Copyright |
Copyright © 1980, 1981-2024 John Wiley & Sons, Inc. All Rights Reserved. |
Dynamic Viscosity |
(Mooney)= (ML-1+4 100C) 43-58 |
Sample Procedure |
The pyrolysis technique is commonly used in the infrared identification of polymers and results in spectra of both the volatile and non-volatile pyrolyzed fractions the polymer under investigation. It can be used by researchers to identify principal polymer types. The volatile (Vapor Phase) and non-volatile (Condensed Phase) IR spectra resulting from the pyrolysis of this sample are available in SpectraBase as EUROPRENE 1707 - Controlled Pyrolyzate (Vapor Phase) and EUROPRENE 1707 - Controlled Pyrolyzate (Condensed Phase). |
Technique |
FILM (CAST FROM o-DICHLOROBENZENE) |