ESCORENE LD-102 HOMOPOLYMER - Controlled Pyrolyzate (Vapor Phase) |
Source of Sample |
Exxon Mobil Corporation |
Chemical Description |
LOW DENSITY POLYETHYLENE RESIN FOR FILM |
Copyright |
Copyright © 1980, 1981-2024 John Wiley & Sons, Inc. All Rights Reserved. |
Density |
0.922 G/CC |
Dynamic Viscosity |
Melt Index= 6.5 G/10 MIN. |
Melting Point |
109.5C |
Sample Procedure |
The pyrolysis technique is commonly used in the infrared identification of polymers and results in spectra of both the volatile and non-volatile pyrolyzed fractions the polymer under investigation. It can be used by researchers to identify principal polymer types. This record contains the volatile (Vapor Phase) IR spectrum resulting from the pyrolysis of ESCORENE LD-102 HOMOPOLYMER. The IR spectrum of the non-volatile (Condensed Phase) fraction resulting from the pyrolysis of ESCORENE LD-102 HOMOPOLYMER is ESCORENE LD-102 HOMOPOLYMER - Controlled Pyrolyzate (Condensed Phase). The Temperature in this record is the temperature of the pyrolysis. |
Technique |
Vapor Phase |