Density |
(Specific Gravity)= (25/15.6C) 1.075 |
Fire Point |
(COC) 470F |
Flash Point |
(COC) 412F |
Optical Properties |
Index of Refraction= (25C) 1.5981 |
Sample Procedure |
The pyrolysis technique is commonly used in the infrared identification of polymers and results in spectra of both the volatile and non-volatile pyrolyzed fractions the polymer under investigation. It can be used by researchers to identify principal polymer types. This record contains the non-volatile (Condensed Phase) IR spectrum resulting from the pyrolysis of CUMAR R-16 (FORMERLY CUMAR MH-2 1/2 RESIN). The IR spectrum of the volatile (Vapor Phase) fraction resulting from the pyrolysis of CUMAR R-16 (FORMERLY CUMAR MH-2 1/2 RESIN) is CUMAR R-16 (FORMERLY CUMAR MH-2 1/2 RESIN) - Controlled Pyrolyzate (Vapor Phase). |
Softening Point |
(RING & BALL) 103C |
Technique |
Condensed Phase |
Values |
Iodine Value= 9 |