SpectraBase Spectrum ID |
28wG4ju7OdF |
Name |
XENOY CX-1100 - Controlled Pyrolyzate (Vapor Phase) |
Source of Sample |
General Electric Company |
Chemical Description |
THERMOPLASTIC POLYMER ALLOY |
Copyright |
Copyright © 1980, 1981-2024 John Wiley & Sons, Inc. All Rights Reserved. |
Density |
(Specific Gravity)= 1.22 |
Sample Procedure |
The pyrolysis technique is commonly used in the infrared identification of polymers and results in spectra of both the volatile and non-volatile pyrolyzed fractions the polymer under investigation. It can be used by researchers to identify principal polymer types. This record contains the volatile (Vapor Phase) IR spectrum resulting from the pyrolysis of XENOY CX-1100. The IR spectrum of the non-volatile (Condensed Phase) fraction resulting from the pyrolysis of XENOY CX-1100 is XENOY CX-1100 - Controlled Pyrolyzate (Condensed Phase). The Temperature in this record is the temperature of the pyrolysis. |
Technique |
Vapor Phase |