SpectraBase Spectrum ID |
1oiNrqxmCzh |
Name |
ST POLYSULFIDE RUBBER - Controlled Pyrolyzate (Condensed Phase) |
Source of Sample |
Thiokol Corporation, Chemical Division |
Chemical Description |
POLYSULFIDE RUBBER |
Copyright |
Copyright © 1980, 1981-2024 John Wiley & Sons, Inc. All Rights Reserved. |
Density |
(Specific Gravity)= 1.27 |
Dynamic Viscosity |
(Mooney)= (ML 1+3 212F) 27-35 |
Sample Procedure |
The pyrolysis technique is commonly used in the infrared identification of polymers and results in spectra of both the volatile and non-volatile pyrolyzed fractions the polymer under investigation. It can be used by researchers to identify principal polymer types. This record contains the non-volatile (Condensed Phase) IR spectrum resulting from the pyrolysis of ST POLYSULFIDE RUBBER. The IR spectrum of the volatile (Vapor Phase) fraction resulting from the pyrolysis of ST POLYSULFIDE RUBBER is ST POLYSULFIDE RUBBER - Controlled Pyrolyzate (Vapor Phase). |
Technique |
Condensed Phase |